High Phosphorus
Roughly 10 to 13 percent phosphorus. The most corrosion resistant option and essentially nonmagnetic, chosen for parts exposed to moisture, salt and chemicals.
Electroless nickel is deposited through an autocatalytic chemical reaction, rather than by passing electrical current through the part. This can support consistent coating build on surfaces reached by the solution. The practical limit is geometry: enclosed cavities and restricted passages need review before coverage can be assumed.
Specify the finish around the part's actual function.
Because the deposit forms chemically, the process does not rely on electrical current to distribute metal over the workpiece. This makes solution access the key geometry question. Show bores, recesses and internal channels on the drawing, especially where they are part of the required coated area.
Phosphorus content changes the deposit's property balance. Low-, medium- and high-phosphorus options should be considered against the expected corrosion exposure, hardness and wear demands. PTFE composite or heat treatment may be discussed when the application supports those options.
Preparation is substrate-specific. Provide the exact alloy designation, any existing finish, the drawing, quantity and required thickness. Steel, stainless steel, aluminum and copper alloys should not be treated as interchangeable materials.
Send us the drawing or a few photos, the material, and what the part does in service. If your print calls out a coating specification or a finished dimension, include it. We will recommend a phosphorus range and a thickness, tell you whether masking or heat treatment makes sense, and send back a written quote.
Available specifications include low-, medium- and high-phosphorus deposits. The review can also consider PTFE composite, masking and post-plating heat treatment when the part's material and requirements support those options.
Roughly 10 to 13 percent phosphorus. The most corrosion resistant option and essentially nonmagnetic, chosen for parts exposed to moisture, salt and chemicals.
Roughly 5 to 9 percent phosphorus. The general purpose workhorse, with a bright appearance and a balance of hardness, wear and corrosion protection that suits most industrial parts.
Roughly 1 to 5 percent phosphorus. The hardest deposit as plated, selected for sliding surfaces, tooling and components where wear resistance matters more than chemical exposure.
A bake after plating can raise hardness to a level that competes with hard chrome, or relieve hydrogen in high strength steel. The cycle is matched to the chemistry and the base metal.
Fine PTFE particles locked into the nickel matrix create a dry lubricating surface. Used on molds, fasteners, sliding mechanisms and anything that needs low friction or easy release.
Internal passages, blind holes, fine threads and deep pockets get the same coating as the outside of the part. Often the only practical choice when conventional plating cannot reach.
We run all three of these processes in house, so we have no reason to push one over another. Here is how they differ and when each one is the right call.
The plating bath is the same for every part. The preparation is not. Each substrate has its own cleaning and activation sequence, and getting it right is what keeps the coating attached.
The most common substrate we coat. After degreasing and acid activation, steel accepts every phosphorus range. High strength steels can receive a hydrogen relief bake after plating.
Its passive oxide film blocks adhesion, so it gets a nickel strike before the electroless bath. Often coated to stop galling on threads or to add surface hardness.
Aluminum oxidizes within seconds, so it receives a zincate treatment that protects the surface until the nickel takes over. The alloy matters, so tell us the grade if you know it.
Copper does not start the reaction on its own, so it is activated before plating. Electroless nickel then acts as a durable barrier against tarnish and diffusion.
Valve bodies, fittings and marine components plate cleanly once activated. The nickel layer protects against dezincification and adds a harder working surface.
Nickel alloys, tool steels and cast parts can be coated case by case. Send the exact alloy designation so we can confirm the activation sequence before you ship.
Everything we offer around electroless nickel, from the chemistry itself to masking, stripping and post plate treatment.
First, the material grade and surface condition are identified. The drawing is then reviewed for solution access, critical dimensions and areas that require masking before a preparation route is selected.
Send photos or a drawing, the material, the quantity and any coating callout on your print.
We suggest a phosphorus range and thickness and send a written quote within 24 business hours.
After the quote and process scope are approved, confirm the receiving instructions before dispatch. Wrap precision faces separately, keep loose parts from contacting one another and include the order reference and packing list. Use separate bags for small pieces and keep the labels visible so receiving can reconcile the shipment with the packing list.
Parts are degreased, masked where needed, activated for their alloy and plated in a controlled bath.
Coverage and thickness are checked, any heat treatment is completed, and parts ship back insured.
From custom builders to industrial manufacturers, our clients trust us to deliver the same result every time.
Fabricators and equipment teams may evaluate a coating for pump housings and fluid-control bodies, but the required properties can differ by end use. A fluid-contact component and a close-fit assembly should not be specified in the same way. These are illustrative applications, not claims of local customer work. The deciding factor is whether the coating must address chemical exposure, mechanical contact or a dimensional requirement.
CNC parts with tight tolerances, where the coating has to go on evenly so the part still fits after plating.
Valves, pump housings, shafts and fixtures that need corrosion protection inside passages as well as outside.
Brackets, fuel system fittings, brake parts and engine components protected from heat, fluids and road salt.
Fittings, pump parts and deck components where high phosphorus nickel stands up to constant salt exposure.
Plastic injection molds, dies and fixtures that need a hard surface, clean release and protection from corrosion.
Threaded parts, hinges and fittings coated all the way into the threads for smooth assembly and lasting protection.
Drag the handle on any photo to compare the part as it arrived with the finished electroless nickel surface.
Before
Arrived with surface rust and a failed zinc finish. Stripped, cleaned and activated, then coated with medium phosphorus nickel for an even, corrosion resistant surface that kept the part within its fit.
Before
Dull, oxidized housings with threaded ports. Each piece went through a zincate pretreatment and received high phosphorus nickel that reached every port and internal face.
Before
Deep pockets and cross drilled passages that conventional plating could not reach evenly. Electroless nickel coated the inside and the outside at the same thickness.
Big order or a single knob, same care.
Homeowners send us one faucet. Companies in and out of state send production runs of hundreds or thousands of parts. Both get a written quote and the same inspection before anything ships back.
Functional plating only counts if the part works when it goes back into the assembly. That is the standard we inspect to on every order.
Bath chemistry, temperature and nickel content are monitored throughout the run so the deposit stays consistent from the first part to the last.
Steel, stainless and aluminum each follow their own cleaning and activation sequence, which is what keeps the coating bonded.
Coverage and coating thickness are checked against your requirement before parts are released for packing.
Finished parts are separated and packed so threads, sealing faces and machined surfaces arrive exactly as they left the tank.
Since 1989 we have plated parts for machine shops, manufacturers, restorers and builders. Decorative work and functional coatings run under the same roof, with the same inspection standard.
Send a photo or drawing and receive a no obligation quote within 24 hours.
Every part leaves our shop backed by our craftsmanship guarantee. If you are not satisfied, we make it right.
Single prototypes or full production runs, shipped to us from any state and returned insured.
Most projects are completed within 3 to 5 weeks. Expedited Orders: 5 to 7 business days. Contact us for availability.
Protect the surfaces that control fit.
Separate finished components during storage and transport. Threads, bores, sealing faces and precision edges should not rub against loose parts or hard packaging. For this part, keep the packaging reference with the component until receiving inspection is complete.
Cleaning and maintenance should follow the equipment requirements and the actual exposure conditions. Do not assume every abrasive method or chemical cleaner is compatible with the part. During assembly, verify that protective packaging has been removed without dragging tools across coated faces.
Thickness is the other key number. Electroless nickel builds evenly, so the coating adds the same amount to every surface, inside diameters included. On a precision fit, that growth has to be planned for. Let us know the finished dimension you need, and whether any threads, bores or sealing faces should be masked and left bare.
Finally, mention quantity and timing. A single prototype and a recurring production run are scheduled differently, and knowing what is coming next lets us hold the same settings from batch to batch.
Electroless Nickel Gallery
Uniform electroless nickel on machined, threaded and complex parts, from valve bodies and molds to marine fittings and hardware.
Decorative Metal Coatings processes electroless nickel orders at its Oceanside, California facility. Eligible projects from El Monte, CA, and elsewhere in the United States may be shipped after the quote and receiving instructions are confirmed. Protect precision surfaces and identify each part number.
Send photos or drawings, the material and the quantity. You receive a written quote and lead time, usually the same business day. Always wait for a quote number before shipping.
Bag or wrap each part separately, cap threads and ports when you can, and keep parts from rubbing against each other. Use plenty of padding on every side of the box.
Declare the real value with the carrier and email us the tracking number so we can log your parts the day they arrive.
Once plating and inspection are complete, we pack the parts in clean materials and ship them back insured, or hold them for pickup.
Every electroless nickel order is cleaned, plated and inspected in our own facility in North County San Diego.
Electroless nickel, chrome and metal finishing in San Diego County since 1989.
Decorative Metal Coatings performs plating and inspection at its facility in Oceanside, California. Eligible projects from other U.S. locations can be shipped for review and processing.
Other cities appearing in the supplied service-area list include:
Frequently Asked Questions
These answers cover coating chemistry, substrate review, dimensions and practical details that can help define a plating request.
It may coat an internal bore when the plating solution can enter, reach the surface and exchange during processing. Provide the bore diameter, depth and whether it is open or blind so access can be evaluated.
It can be selected for corrosion-related requirements, but results depend on deposit chemistry, thickness, substrate preparation, geometry and exposure. Describe the actual environment and any test standard.
Added deposit can change thread dimensions and engagement. Identify the thread specification and finished-fit requirement, and show whether threads should be coated or masked.
Yes. Separate appearance expectations from functional requirements such as thickness, corrosion protection or fit. This helps the review focus on the acceptance criteria that matter.
It may be possible, but list each part number with its own drawing and thickness requirement. Clear identification helps prevent different specifications from being applied to the wrong components.
Send us a few photos of the part from different angles, along with what it is and the finish you want. We look them over and send a written quote, usually within 24 business hours. It's free, and you're under no obligation to go ahead.
Standard orders take 3 to 5 weeks from the day your parts arrive. If you're on a deadline, ask about expedited service. When the schedule allows, we can finish in 5 to 7 business days.
Yes. Our workmanship is covered for 12 months. If something isn't right with the finish we put on, call us and we'll make it right.